High-temperature investment · Water mix
MAGNAVEST™PT
High-temperature casting.
Just add water.
A premium phosphate bonded investment for platinum, palladium, stainless steel and chrome cobalt alloys. Mixes easily with water to form a smooth, consistent slurry.
- 10 kg Aluminum vacuum-sealed sack
MAGNA VEST PT is available only in 10 kg aluminum vacuum-sealed sacks.
01 / The MAGNA VEST PT difference
Simple preparation.
Precise results.
MAGNA VEST PT is a high-temperature phosphate bonded investment developed for platinum, palladium, stainless steel and chrome cobalt alloys. Its user-friendly formula combines water-only preparation with stable performance throughout burnout.
A straightforward water mix.
Consistency from batch to batch.
Sharp detail. Less finishing.
PREPARE YOUR BATCH
Your mix.
Calculated.
Water only · method-specific quantities · 10–15°C
Enter the weight of dry powder.
1 kg powder × 0.28 = water in liters
No binder concentrate required.
- 01 · PREPARE
Weigh powder & water
Measure the calculated water at 10–15°C and weigh the MAGNA VEST PT powder.
- 02 · IN THIS ORDER
Add powder to water
Always add powder to the measured water.
- 03 · 4–5 MIN
Mix under vacuum
Mix and vacuum together for 4–5 minutes.
- 04 · 1 MIN
Pour into the flask
Fill the prepared flask within 1 minute.
- 05 · 2 MIN
Vacuum the flask
Vacuum the filled flask for 2 minutes.
- 06 · 180–240 MIN
Allow to stand
Leave undisturbed for 180–240 minutes (3–4 hours) before burnout.
Water quantity and working time follow the selected method. Keep water at 10–15°C and leave the flask undisturbed for 3–4 hours before burnout. Ask our technical team ↗
03 / Injection-wax burnout cycle
Five plateaus.
Controlled progression.
The catalog injection-wax program progresses through five temperature plateaus to 900°C. Select a ramp or hold below to follow the cycle.
The time under each temperature is the hold at that temperature.
Swipe the chart to see the complete program →
| Target temperature | Time to reach target | Hold at target |
|---|---|---|
| 110 °C | ||
| 300 °C | ||
| 720 °C | ||
| 850 °C | ||
| 900 °C | ||
Cooling: no fixed duration is specified; follow the temperature required by your casting process.
110°C → 300°C → 720°C → 850°C → 900°C. The dashed cooling segment is illustrative; the final temperature depends on your casting process.
Injection-wax program · Burnout time may vary with flask size. Technical support ↗
Your next casting
Let’s make every
detail count.
Discuss MAGNA VEST PT, your casting process or your next order with the PRESTIGE team.