Logo — PRESTIGE
PRESTIGE / Investment powders / OROPrecision begins with preparation.

Ultra-premium investment

ORO™

For palladium, yellow
and white gold up to 22K.

A smooth, creamy mix. Investment engineered to preserve the finest details of your casting.

Calculate your mix
ORO — PRESTIGE
  • 22.5 kg Plastic-lined poly sack
  • 22.5 kg Ergonomic plastic drum
  • 45 kg Heavy-duty reusable plastic drum

The reusable drums can also provide containment for used investment.

Investment typeGypsum bonded
Gold castingUp to 22K gold
Formulation focusFine detail. Smooth surfaces.
ORO – The difference is in the detail — PRESTIGE
From the ORO catalog · Detail, reproduced.

01 / The ORO difference

The difference
is in the detail.

ORO is an ultra-premium gypsum bonded investment developed and perfected for casting gold up to 22K.

  1. A finer surface, from the start.

  2. A mix that works with you.

  3. Less work after the casting.

Controlled expansion · Consistent from batch to batch

PREPARE YOUR BATCH

Your mix.
Calculated.

Catalog range: 38–40%. Additional setting: 37%.

Choose your water ratio
kg

Enter the weight of dry powder.

WATER REQUIRED
0.38 liters

1 kg powder × 0.38 = water in liters
100 parts powder : 38 parts water

Water 21–24°CWorking time 8 min
  1. 01

    Weigh & prepare

    Measure the calculated water at 21–24°C and weigh your ORO powder.

  2. 02

    Add powder to water

    Always add powder to the measured water, in that order.

  3. 03 · 4–5 MIN

    Mix under vacuum

    Mix and vacuum together for 4–5 minutes.

  4. 04 · 2 MIN

    Pour into the flask

    Fill the prepared flask within 2 minutes.

  5. 05 · 1 MIN

    Vacuum the flask

    Vacuum the filled flask for 1 minute.

  6. 06 · 90–120 MIN

    Leave undisturbed

    Allow the flask to stand for 90–120 minutes before burnout.

Choose your water ratio. Ask our technical team ↗

03 / Recommended burnout cycle

Controlled heat.
Prepared for precision.

The standard ORO cycle, from the first temperature rise to the final hold. Select a stage below to follow the program.

ORO · STANDARD CYCLE13 hours to complete the peak hold

The time under each temperature is the hold at that temperature.

ORO standard burnout program Ramp to 150 degrees Celsius in 1 hour, hold 3 hours. Ramp to 370 in 1 hour, hold 2 hours. Ramp to 750 in 2 hours, hold 4 hours. Then cool to the required flask temperature for casting. The cooling segment is schematic; no cooling time or casting temperature is specified. 8006004002000°C01457913TIME IN HOURS 150 °C3 h370 °C2 h750 °C4 h

Swipe the chart to see the complete program →

Injection wax
Target temperatureTime to reach targetHold at target
150 °C
370 °C
750 °C

Cooling: no fixed duration is specified; follow the temperature required by your casting process.

150°C → 370°C → 750°C. The dashed cooling line is illustrative; the final temperature depends on your casting process.

Standard ORO cycle · Technical support ↗

Your next casting

Let’s make every
detail count.

Discuss ORO, your casting process or your next order with the PRESTIGE team.

+90 212 674 81 47

PRESTIGE / ORO

Let’s talk about ORO.

Tell our team about your casting process or your next order.

We’ll use your details to respond to your inquiry.

Open in email app chris@certus-int.com

Prefer email? chris@certus-int.com

Contact us

Choose your language

Select a language. You will stay on this page.

EnglishРусскийEspañolDeutsch简体中文ItalianoالعربيةBahasa Indonesiaहिन्दीTürkçePortuguês (Portugal)ไทยFrançaisاردوفارسیO‘zbekchaTiếng ViệtPortuguês (Brasil)