Precision for tire mold casting
POWERCAST “T”
For the detail
behind every tread.
A non-foamed investment molding plaster developed for aluminum alloy casting. Engineered for the precise, complex tread patterns of tire vulcanization molds.
- 22.5 kg Plastic-lined poly sack
- 1 metric ton Heavy-duty bulk bag
Choose individual sacks or heavy-duty bulk bags to match your production volume.
01 / The POWERCAST “T” difference
Every groove.
Every detail.
POWERCAST “T” is a non-foamed, gypsum bonded investment molding plaster developed for casting aluminum alloys for tire mold production. It reproduces intricate tread configurations for molds used in tire vulcanization.
Precision in every tread.
A smoother casting surface.
Consistency through production.
PREPARE YOUR BATCH
Your mix.
Calculated.
Method-specific water quantities · 21–24°C
Enter the weight of dry powder.
1 kg powder × 0.50 = water in liters
- 01 · Prepare
Weigh powder & water
Measure the calculated water at 21–24°C and weigh the POWERCAST “T” powder.
- 02 · In this order
Add powder to water
Add the powder to the measured water.
- 03 · 4–5 min
Mix under vacuum
Mix and vacuum together for 4–5 minutes.
- 04 · 3 min
Pour into the mold
Pour the mixed investment into the mold flask over 3 minutes.
- 05 · 3 min
Vacuum the mold
Vacuum the filled mold flask for 3 minutes.
- 06 · 120–150 min
Allow to stand
Leave undisturbed for 120–150 minutes before burnout.
After the 11-minute working sequence, leave the filled mold undisturbed for 120–150 minutes before burnout. Measure accurately: a 1% increase in powder can shorten working time by approximately 30 seconds. Ask our technical team ↗
03 / Recommended burnout cycle
The tire-mold cycle.
Every stage in view.
The POWERCAST “T” catalog program has two plateaus: 150°C and 295°C. Select a stage below to follow the cycle. Burnout time may vary with flask size.
The time under each temperature is the hold at that temperature.
Swipe the chart to see the complete program →
| Target temperature | Time to reach target | Hold at target |
|---|---|---|
| 150 °C | ||
| 295 °C | ||
Cooling: no fixed duration is specified; follow the temperature required by your casting process.
150°C → 295°C · 24 hours before cooling. Cool to the required flask temperature for casting; the dashed line is schematic and specifies neither a fixed cooling time nor a target temperature.
Program shown: POWERCAST “T” from the PRESTIGE catalog. Need help matching the cycle to your mold size and process? Technical support ↗
Your next casting
Let’s make every
detail count.
Discuss POWERCAST “T”, your tire mold process or your next order with the PRESTIGE team.