Logo — PRESTIGE
PRESTIGE / Investment powders / ROYAL CASTPrecision begins with preparation.

Strength for every casting.

ROYALCAST™

For brass and bronze
jewelry casting.

Strong, stable molds. A smooth, easy-pour mix. Investment developed for detailed brass and bronze castings, from small batches to high-volume production.

Calculate your mix
ROYAL CAST — PRESTIGE
  • 22.5 kg Poly sack with a plastic liner

ROYAL CAST is supplied in a single sack format for brass and bronze casting workshops.

Investment typeGypsum bonded
Recommended metalsBrass · Bronze
Mold performanceHigh green & fired strength
ROYAL CAST – Strong molds. Sharper detail — PRESTIGE
Brass & bronze casting · Detail, reproduced.

01 / The ROYAL CAST difference

Strong molds.
Sharper detail.

ROYAL CAST is a high-quality, cost-effective gypsum bonded investment developed for brass and bronze jewelry. Specially graded refractory minerals and control additives support sharp surface detail and consistent results in both low- and high-volume workshops.

  1. A smooth, controlled mix.

  2. Strength throughout the process.

  3. Detail made for brass and bronze.

38–40% water / powder · Thick to fine designsHigh green & fired strength · Thermal shock resistance

PREPARE YOUR BATCH

Your mix.
Calculated.

Catalog range: 38–40%. Additional setting: 37%.

Choose your water ratio
kg

Enter the weight of dry powder.

WATER REQUIRED
0.38 liters

1 kg powder × 0.38 = water in liters
100 parts powder : 38 parts water

Water 21–24°CWorking time 8 min
  1. 01

    Weigh & prepare

    Measure the calculated water at 21–24°C and weigh your ROYAL CAST powder.

  2. 02

    Add powder to water

    Always add powder to the measured water, in that order.

  3. 03 · 4–5 MIN

    Mix under vacuum

    Mix and vacuum together for 4–5 minutes.

  4. 04 · 2 MIN

    Pour into the flask

    Fill the prepared flask within 2 minutes.

  5. 05 · 1 MIN

    Vacuum the flask

    Vacuum the filled flask for 1 minute.

  6. 06 · 90–120 MIN

    Leave undisturbed

    Allow the flask to stand for 90–120 minutes before burnout.

Choose your water ratio. Ask our technical team ↗

03 / Recommended burnout cycle

Controlled heat.
Prepared for precision.

The standard ROYAL CAST cycle, from the first temperature rise to the final hold. Select a stage below to follow the program.

ROYAL CAST · STANDARD CYCLE13 hours to complete the peak hold

The time under each temperature is the hold at that temperature.

ROYAL CAST standard burnout program Ramp to 150 degrees Celsius in 1 hour, hold 3 hours. Ramp to 370 in 1 hour, hold 2 hours. Ramp to 730 in 2 hours, hold 4 hours. Then cool to the required flask temperature for casting. The cooling segment is schematic; no cooling time or casting temperature is specified. 8006004002000°C01457913TIME IN HOURS 150 °C3 h370 °C2 h730 °C4 h

Swipe the chart to see the complete program →

Injection wax
Target temperatureTime to reach targetHold at target
150 °C
370 °C
730 °C

Cooling: no fixed duration is specified; follow the temperature required by your casting process.

150°C → 370°C → 730°C. The dashed cooling line is illustrative; the final temperature depends on your casting process.

Standard ROYAL CAST cycle · Technical support ↗

Your next casting

Let’s make every
detail count.

Discuss ROYAL CAST, your casting process or your next order with the PRESTIGE team.

+90 212 674 81 47

PRESTIGE / ROYAL CAST

Let’s talk about ROYAL CAST.

Tell our team about your casting process or your next order.

We’ll use your details to respond to your inquiry.

Open in email app chris@certus-int.com

Prefer email? chris@certus-int.com

Contact us

Choose your language

Select a language. You will stay on this page.

EnglishРусскийEspañolDeutsch简体中文ItalianoالعربيةBahasa Indonesiaहिन्दीTürkçePortuguês (Portugal)ไทยFrançaisاردوفارسیO‘zbekchaTiếng ViệtPortuguês (Brasil)