One investment. Multiple applications.
UNICAST™
For yellow and white
gold up to 18K.
Reliable, everyday performance. A thin, creamy mix for detailed castings in gold, sterling silver, fine silver and bronze.
- 22.5 kg Plastic-lined poly sack
- 22.5 kg Ergonomic plastic drum
- 45 kg Heavy-duty reusable plastic drum
The reusable drums can also provide containment for used investment.
01 / The UNICAST difference
One investment.
More possibilities.
UNICAST is a premium gypsum bonded investment for workshops that prefer one formula for multiple casting applications. Designed for gold up to 18K, it also supports complex designs in sterling silver, fine silver and bronze.
Versatility for your workshop.
Easy to mix. Easy to pour.
Consistency through to clean-up.
PREPARE YOUR BATCH
Your mix.
Calculated.
Catalog range: 38–40%. Additional setting: 37%.
Enter the weight of dry powder.
1 kg powder × 0.38 = water in liters
100 parts powder : 38 parts water
- 01
Weigh & prepare
Measure the calculated water at 21–24°C and weigh your UNICAST powder.
- 02
Add powder to water
Always add powder to the measured water, in that order.
- 03 · 4–5 MIN
Mix under vacuum
Mix and vacuum together for 4–5 minutes.
- 04 · 2 MIN
Pour into the flask
Fill the prepared flask within 2 minutes.
- 05 · 1 MIN
Vacuum the flask
Vacuum the filled flask for 1 minute.
- 06 · 90–120 MIN
Leave undisturbed
Allow the flask to stand for 90–120 minutes before burnout.
Choose your water ratio. Ask our technical team ↗
03 / Recommended burnout cycle
Controlled heat.
Prepared for precision.
The standard UNICAST cycle, from the first temperature rise to the final hold. Select a stage below to follow the program.
The time under each temperature is the hold at that temperature.
Swipe the chart to see the complete program →
| Target temperature | Time to reach target | Hold at target |
|---|---|---|
| 150 °C | ||
| 370 °C | ||
| 750 °C | ||
Cooling: no fixed duration is specified; follow the temperature required by your casting process.
150°C → 370°C → 750°C. The dashed cooling line is illustrative; the final temperature depends on your casting process.
Standard UNICAST cycle · Technical support ↗
Your next casting
Let’s make every
detail count.
Discuss UNICAST, your casting process or your next order with the PRESTIGE team.